A fish cage net may be manufactured from one continuous panel with the same:
Mesh size
Twine construction
Knot type
Material
Production batch
Yet after installation, the mesh openings near the surface may look different from those in the middle or near the bottom.
Some openings may appear:
Wider
Narrower
Taller
Shorter
More diagonal
Less regular
This does not automatically mean the net was manufactured with different mesh sizes.
In many cases, the difference comes from how the flexible mesh is loaded underwater.
The key principle is:
The nominal mesh may be the same throughout the panel, while the effective opening changes because each depth experiences different tension, geometry, and environmental load.
A diamond-shaped mesh does not have one fixed width and height.
When pulled vertically, it becomes taller and narrower.
When pulled horizontally, it becomes wider and shorter.
Therefore, two sections made from identical mesh can show different clear openings simply because they are tensioned in different directions.
The top section is usually close to:
Floating collars
Frames
Border ropes
Attachment loops
These structures restrict movement.
If the upper border is tightly attached, the nearby mesh may be pulled more horizontally.
This can make the openings appear wider and shorter than deeper sections.
The center of a side panel is usually farther from rigid support.
Under current, it can bow downstream more freely.
As the panel curves, mesh angles change.
The result may be a different opening shape from both the top and bottom sections.
The lower net is affected by:
Sinker ropes
Sinker tubes
Bottom weights
Bottom-panel tension
Vertical loading can make some lower mesh openings taller and narrower.
If sinker weight is uneven, mesh size may also vary from one lower section to another.
A heavy sinker point pulls nearby mesh more strongly.
A section between widely spaced sinkers may remain looser or rise under current.
This creates alternating:
Tight mesh
Loose mesh
Different opening angles
The original mesh side length may still be the same.
Water movement is not always uniform from surface to bottom.
Different depths may experience different:
Current speed
Direction
Turbulence
Wave influence
This changes how strongly each part of the panel is pushed.
The upper section experiences repeated movement from waves and floating-frame motion.
This can cause rapid cycles of:
Tightening
Relaxation
Mesh rotation
Knot movement
Lower sections may move more slowly.
Over time, the upper and lower mesh may no longer sit in exactly the same geometry.
In coastal aquaculture, current direction may reverse.
A mesh opening stretched in one direction during one tide may rotate in the opposite direction later.
This repeated movement can create local differences in:
Knot seating
Twine tension
Mesh recovery
Biofouling does not grow uniformly.
The surface, middle, and lower zones may have different levels of:
Algae
Slime
Mussels
Barnacles
Other organisms
A heavily fouled section has less effective open area and greater drag.
This changes how the surrounding mesh is loaded.
The manufactured mesh opening may remain unchanged, but fouling physically occupies part of the opening.
This means there are two different concepts:
Manufactured Mesh Size
and
Effective Water-Flow Opening
A 25 mm nominal opening, for example, may provide much less clear water passage after heavy fouling.
Deep and bottom sections may accumulate heavier shell growth or sediment.
Additional weight pulls the mesh downward.
This can make lower openings appear more vertically elongated.
If the upper section is cleaned frequently but the lower section remains fouled, the two zones behave differently.
The cleaned section becomes:
Lighter
More flexible
More permeable
The fouled section remains:
Heavier
Stiffer
Higher in drag
The transition between them may develop visibly different mesh geometry.
Vertical borders may not carry uniform tension from top to bottom.
Differences can result from:
Attachment spacing
Border elongation
Sinker weight
Knot settling
A tight lower border and loose middle section can create different mesh openings along the same panel.
Mesh close to an attachment loop is usually more restrained.
Mesh halfway between two attachments can move more freely.
Therefore, even at the same depth, openings may vary depending on distance from the nearest support.
This is why sampling only one mesh is unreliable.
Corners usually contain:
Reinforced borders
Attachment loops
Extra knots
More concentrated load
Mesh near a corner may be more stretched or skewed than mesh in the center.
When comparing different depths, the sampling position should also be consistent horizontally.
A repair patch may have different:
Twine diameter
Mesh tension
Knot tightness
Flexibility
A tight patch can make nearby openings smaller.
A loose patch can allow them to become larger or more irregular.
Repeated tension can cause some knots to:
Settle
Rotate
Slip slightly
This may release twine into one opening while shortening another.
The result is local mesh-size variation even though no row has been added or removed.
Synthetic twine under sustained tension may gradually deform over time.
The amount depends on:
Material
Load
Temperature
Construction
Service duration
Creep may be greater in heavily loaded sections, so different depths can gradually develop different geometry.
Upper and waterline sections generally receive more sunlight than deep submerged mesh.
Long-term UV exposure can change:
Flexibility
Elongation
Surface condition
This means the same tension may produce different deformation in aged upper twine compared with less-exposed lower twine.
Before concluding that different depths contain different mesh sizes, confirm the measurement method.
Possible methods include:
Knot-to-knot
Stretched mesh
Clear opening
Do not compare a relaxed underwater opening with a fully stretched factory measurement.
The measurement condition must be defined.
One opening may be distorted by a knot or local load.
For better comparison:
Select a defined zone.
Measure several consecutive openings.
Use the same tension.
Record the average and range.
Repeat at other depths.
This provides a more representative result.
For example, compare:
Upper center
Middle center
Lower center
rather than comparing an upper corner with the lower center.
This helps separate the effect of depth from the effect of structural position.
Mesh geometry changes with water movement.
Measurements made during strong current should not be directly compared with measurements taken during slack water unless the operating condition is part of the analysis.
Uneven effective mesh size can influence:
Water exchange
Fish containment
Fish behavior
Drag
Local tension
Cleaning efficiency
It may also indicate underlying problems such as:
Uneven sinkers
Attachment imbalance
Fouling
Border distortion
Repair tension
Avoid strong local vertical pull.
Reduce unsupported spans.
Do not over-tighten upper borders.
Avoid large clean–fouled differences.
Detect local slippage or rotation.
Avoid stiff or overly tight patch boundaries.
Track changes at the same locations over time.
Compare:
✔ Upper panel
✔ Waterline
✔ Middle panel
✔ Lower panel
✔ Bottom area
Check:
✔ Mesh opening shape
✔ Knot-to-knot dimension
✔ Mesh orientation
✔ Twine tension
✔ Fouling level
✔ Attachment spacing
✔ Sinker distribution
✔ Border condition
✔ Repair locations
✔ Current direction
Warning signs:
✔ Very wide upper openings
✔ Tall narrow lower openings
✔ Sudden change between two depths
✔ Skewed mesh around attachments
✔ Mesh distortion beside repairs
✔ Large differences after partial cleaning
The same fishing net can have different mesh openings at different depths because each part of the panel experiences a different combination of:
Current
Wave motion
Vertical load
Sinker tension
Fouling
Attachments
UV exposure
Repairs
The key principle is:
The manufactured mesh specification may remain the same, while the effective opening changes with local geometry and operating load.
Reliable evaluation combines:
Consistent Mesh Measurement + Depth-Based Sampling + Sinker and Attachment Inspection + Fouling Control + Observation Under Current
At PL Fishery, we manufacture PE fishing nets, fish cage panels, aquaculture netting, reinforced borders, attachment loops, bottom netting, repair mesh, repair twine, marine ropes, chicken nets, and customized net products.
To purchase or customize fishing netting, send PL Fishery your required mesh size and measurement method, twine construction, panel dimensions, cage depth, attachment spacing, sinker system, operating current, fouling conditions, and dimensional tolerances so our factory can prepare a measurable production and inspection specification.